Advanced Prototyping offers a wide variety of prototype material options for your project. The technologies associated with rapid prototyping/3D printing (SLS, SLA, etc.) are fairly well known, the growing array of materials available can be a difficult to puzzle to put together. To help our customers choose wisely, the API rapid protoytping materials guide is a quick one page reference tool showing material and physical properties and metrics of SLA materials, SLS materials, and urethane materials for your parts. For custom blends and other materials, call API and we'll find the appropriate specialty prototyping material for your project.

The design features of your application will determine the material used. Most of the materials used are specialized plastics such as polypropylene, nylon, epoxy resins, and urethane. API can ensure that the right 3D prototyping process and material are selected, no matter what your application for the end-use parts.

 

SLA Materials - Stereolithography

Click on the links to download PDFs.

SLA/Rigid - Accura-55 White
Simulate the look and feel of molded ABS with this tough and versatile plastic.

  • Automotive interior parts
  • Rigid and durable functional rapid prototypes
  • Short-run production parts
  • Concept and marketing models
  • Electronic components
  • Accurate, durable master patterns for urethane casting
  • Testing of functional assemblies

Technical Data

Liquid Material

Measurement Condition Value
Appearance White
Liquid Density @ 25 °C (77 °F) 1.13 g/cm³
Solid Density @ 25 °C (77 °F) 1.20 g/cm³
Viscosity @ 30 °C (86 °F) 155 - 185 cps
Penetration Depth (Dp)* 5.2 mils
Critical Exposure(Ec)* 7.4 mJ/cm²
Tested Build Styles EXACT™, FAST™, EXACT™ HR

Post-Cured Material

Measurement Condition Metric U.S.
Tensile Strength ASTM D 638 63 - 68 MPa 9,200 - 9,850 PSI
Tensile Modulus ASTM D 638 3,200 - 3,380 MPa 460 - 490 KSI
Elongation at Break (%) ASTM D 638 5 - 8 % 5 - 8 %
Flexural Strength ASTM D 790 88 - 110 MPa 12,830 -15,920 PSI
Flexural Modulus ASTM D 790 2,690 - 3,240 MPa 390 - 470 KSI
Impact Strength (Notched Izod) ASTM D 256 12 - 22 J/m 0.2 - 0.4 ft-lb/in
Impact Strength (Notched Izod) ASTM D 5420 1.1 J 0.81 ft - lbs
Heat Deflection Temperature ASTM D 648
@ 66 PSI
@ 264 PSI
55 - 58 °C
51 - 53 °C
131 - 136 °F
123 - 127 °F
Hardness, Shore D 85 85
Co-Effcient of Thermal Expansion ASTM E 831-93
TMA (T<Tg, 0-40 °C)
TMA (T<Tg, 75-140 °C)
61 x μm/m -°C
163 μm/m -°C
141 μin/in - °F
326 μin/in - °F
Glass Transition (Tg) DMA, E" 56 °C 132°F

Accura Xtreme Grey

Ultra-tough grey plastic with outstanding durability, accuracy and aesthetics to replace CNC-machined polypropylene and ABS articles.

Fast and easy to process, the Accura Xtreme material offers physical properties that are close enough to durable end-use plastics like ABS and polypropylene to make it ideal for functioning prototypes in demanding applications, as well as for short-run production projects. Accura Xtreme is a grey plastic with the appearance of a final production part with outstanding durability, impact resistance, accuracy and a thermal resistance over 60° C.

Post-Cured Material

Measurement Condition Metric U.S.
Tensile Strength
(MPa)/PSI)
ASTM D 638 38-44 5510-6380
Tensile Modulus
(MPa/KSI)
ASTM D 638 1790-1980 260-287
Elongation at Break (%) ASTM D 638 14-22 14-22
Flexural Strength
(MPa/KSI)
ASTM D 790 57-71 7540-10300
Flexural Modulus
(MPa/KSI)
ASTM D 790 1520-2070 220-300
Impact Strength
(J/m /Ft-lbs/in)
ASTM D 256 35-52 0.66-0.98
Heat Deflection
Temperature
ASTM D 648
@ 66 PSI
@ 264 PSI
62 °C
54 °C
144 °F
129 °F
Glass Transition (Tg)   70-74 °C 158-165 °F

Liquid Material

Measurement Condition Value
Viscosity @ 30 °C (86 °F) 250-300 cps
Penetration Depth (Dp)   4.1 mils
Critical Exposure (Ec)   11.7 mJ/cm2
Color   Grey
Solid Density @ 25 °C (77 °F) 1.19 g/cm3
Liquid Density @ 25 °C (82 °F) 1.13 g/cm3
Tested Build Styles   EXACT™

SLA/Rigid - DSM-10122 Clear

DSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. In SLA rapid prototyping, it produces colorless, functional, accurate parts that simulate acrylic in appearance. Based on the Oxetane Advantage™, the parts also have improved water resistance over the original WaterClear 10120 resin. WaterClear Ultra is a fast, low viscosity, general-purpose resin.

Mechanical Properties (Metric)

ASTM Method Description Somos® WaterClear® Ultra UV Postcure Acrylic
D638M Tensile Strength
Tensile Modulus
Elongation at Break
Elongation at Yield
Poisson's Ratio
55 - 56 MPa
2,860 - 2,900 MPA
6 - 9 %
4 %
0.40 - 0.42
47 - 79 MPa
2,200 - 3,800 MPa
1 - 30 %
4 %
0.37 - 0.45
D790M Flexural Strength
Flexural Modulus
82 - 85 MPa
2,410 - 2,570 MPa
88 - 138 MPa
3,000 - 3,500 MPa
D256A Izod Impact-Notched 0.24 - 0.26 J/cm 0.15 J/cm
D2240 Hardness (Shore D) 86 - 87 63 - 97
D570-98 Water Absorption 1.1 % 0.3 - 2.0 %
D542 Index of Refraction 1.515 1.498

Thermal & Electrical Properties (Metric)

ASTM Method Description Somos® WaterClear® Ultra UV Postcure Acrylic
E831-00 C. T. E. -40°C – 0°C
C. T. E. 0°C – 50°C
C. T. E. 50°C – 100°C
C. T. E. 100°C – 150°C
63.6 - 66.8 μm/m- °C
87.8 - 93.0 μm/m- °C
164.3 - 171.9 μm/m- °C
149.9 - 167.1 μm/m- °C
D150-98 Dielectric Constant 60Hz
Dielectric Constant 1KHz
Dielectric Constant 1MHz
3.0 - 3.2
3.3 - 3.6
3.0 - 3.2
4.0
3.5
3.0
D149-97a Dielectric Strength 14.5 - 15.5 kV/mm 18 - 60 kV/mm
E1545-00 Tg 42 - 46 °C 100 - 105 °C
D648-98c HDT@ 0.46 MPa
HDT @ 1.82 MPa
46 - 47 °C
42 - 43 °C
80 - 103 °C
80 - 103 °C
Thermal postcure
HDT @ 0.46 MPa 59 - 61 °C
HDT @ 0.46 MPa 59 - 61 °C

Mechanical Properties (Imperial)

ASTM Method Description Somos® WaterClear® Ultra UV Postcure Acrylic
D638M Tensile Strength
Tensile Modulus
Elongation at Break
Elongation at Yield
Poisson's Ratio
7.9 - 8.1 ksi
414 - 421 ksi
6 - 8 %
4 %
0.40 - 0.42
6.8 - 11.5 ksi
319 - 551 ksi
1 - 30 %
4 %
0.37 - 0.45
D790M Flexural Strength
Flexural Modulus
11.8 - 12.4 ksi
349 - 373 ksi
12.8 - 20.0 ksi
435 - 508 ksi
D256A Izod Impact-Notched 0.44 - 0.48 ft-lb/in 0.3 ft-lb/in
D2240 Hardness (Shore D) 86 - 87 63 - 97
D570-98 Water Absorption 1.1 % 0.3 - 2.0 %
D542 Index of Refraction 1.515 % 1.498

Thermal & Electrical Properties (Imperial)

ASTM Method Description Somos® WaterClear® Ultra UV Postcure Acrylic
E831-00 C. T. E. -40°F – 32°F
C. T. E. 32°F – 122°F
C. T. E. 122°F – 212°F
C. T. E. 212°F – 302°F
35.3 - 37.1 μin/in- °F
48.8 - 51.7 μin/in- °F
91.3 - 95.5 μin/in- °F
83.3 - 92.9 μin/in- °F
D150-98 Dielectric Constant 60Hz
Dielectric Constant 1KHz
Dielectric Constant 1MHz
3.0 - 3.2
3.3 - 3.6
3.0 - 3.2
4.0
3.5
3.0
D149-97a Dielectric Strength 367 - 393 V/mil 456 - 1520 V/mil
E1545-00 Tg (TMA) 108 - 115°F 212 - 221°F
D648-98c HDT@ 66 psi
HDT @ 264 psi
115 - 116 °F
108 - 110 °F
176 - 217 °F
176 - 217 °F
Thermal postcure
HDT @ 66 psi 139 - 142 °F
HDT @ 264 psi 120 - 122 °F